Table 2.

Technological parameters of boron carbide powder production.

No Sample Raw material Method Crucible sizes, mm Sintering parameters
Tmax, °C Holding time τ, h Cooling time τ, h Pressure, Pa
1 CRP1 H310BO3, 250P WCP, CR, Induct.
sintering
D185×210 1900 2 15 105
2 CRP2 H310BO3, 250P CR, Induct.
sintering
3 CRKS H310BO3, KS6
4 DSI1 11B, P-803 DSE, Induct.
sintering
D80×210 1900 1 8 10−3
5 DSI2 10B, P-803 D185×210 1900 2 15
6 DSI3 10B, P-803 1850 2
7 DSR1 10B, P-803 DSE, Resist.
sintering
D100×210 1800 1 8 10−4
8 DSR2 10B, P-803 1820 1
9 DSR3 10B, P-803 1820 2
10 DSR4 10B, P-803 1800 2
11 DSR5 10B, P-803 1840 1
12 DSR6 10B, P-803 1840 2

Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.

Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.

Initial download of the metrics may take a while.