Fig. 6

Download original image
Three-directional dynamic test performed at SRMD on a full-scale (1350 mm diameter) HDRB. After partial damage occurred close to 300% shear strain (almost three times the design value), the isolator was successfully subjected to a full cycle under the design load at the design conditions.