7Li plot with same data as in Figures 12 (left) and 8 (right). The left plot shows the 7Li distribution in the oxide with normal thickness (8–10 μm) at 180°. The right plot shows the strongly elevated 7Li at the area of rod-to-rod contact (∼35–50 μm oxide thickness).