Table 2
Basic parameters of tested ceramics.
Parking according to ČSN EN 60672 | Symbol | Unit | CORDIERIT C410 |
Corundum ceramics C799 |
---|---|---|---|---|
Commercial name | TH 7/7 R12 BM | Luxal 203 | ||
Porosity | pa | [%] | 0.5 | |
Density | ρa | [g.cm–3] | 2.1 | min. 3.8 |
Bending strength | σ | [MPa] | 60 | min. 300 |
Thermal expansivity coefficient | α30–600 | [10–6K–1] | 2–4 | 7–8 |
Heat conductivity | λ30–10 | [Wm–1K–1] | 1.2–2.5 | |
Resistance against sudden chase of temperature | ΔT | [K] | 250 | min. 150 |
Relative permittivity | εr | [–] | 5 | |
Al2O3 content | % by weight | 33 | min. 99.5 | |
Inner electric resistance at 30, 200 and 600 °C | ρv,30 | [Ω.m] | 1010 | |
ρv,200 | [Ω.m] | 106 | 1012 | |
ρv,600 | [Ω.m] | 103 | 108 |
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.